Aluminum CRATER - Pitting Corrosion

#aluminum #aluminium #aluminumboat #catamaran #corrosion #diy #fyp #highlights #everyone

#aluminum #aluminium #aluminumboat #catamaran #corrosion #diy #fyp #highlights #everyone

Note of Recognition for Sailing Life on Jupiter

At WeBoating.com, we profoundly acknowledge the unwavering dedication that Sailing Life on Jupiter and other creators invests in crafting each and every video. Their passion for delivering exceptional content shines through every frame, and it's a labor of love that deserves your attention.

We invite you to watch their captivating videos and actively engage with their content, including their social media links above. Liking, commenting, and sharing their work goes a long way in fueling their creative fire.

We're also inviting you to explore any sponsorships and partnerships highlighted in the video description of "Aluminum CRATER - Pitting Corrosion", or directly on YouTube. By considering their offerings or purchasing services and items, you not only support Sailing Life on Jupiter but also the brands and collaborators they're associated with.

If you have any feedback, corrections, or additional information about Sailing Life on Jupiter or their videos, please use the comment form below to share your thoughts with us.

Thank you for being a part of our community and supporting the creators we cherish. Your time and support truly matter!

Sailing Life on Jupiter Lastest Videos

Showing 1-24 of 514 results
Our 220V inverter being dramatic while we install the 120V upgrade…
Sailing Life on Jupiter
After 15 years of loyal service, we’re saying goodbye to our MPPT solar controller.
Sailing Life on Jupiter
WELDING ALUMINUM RUDDER – WHAT WENT WRONG?
Sailing Life on Jupiter

WELDING ALUMINUM RUDDER – WHAT WENT WRONG?

If you get value from our videos whether entertainment. education or inspiration show your appreciation by supporting our channel. ▶️Visit Our Website: https://www.sailinglifeonjupiter.com ▶️ SUPPORT US HERE 👇: JOIN our “PRIME” crew on PATR...
UFO skywatch in Sedona with Melinda Leslie. One of the most mind-blowing experiences we’ve had.
Sailing Life on Jupiter
My husband made my birthday unforgettable with this hot air balloon ride in Sedona. 🥰🎈🎂🎉
Sailing Life on Jupiter
Best birthday balloon ever. 🎈🎉#BIRTHDAYGIRL #HotAirBalloon
Sailing Life on Jupiter
This Aluminum Boat Project Just Got Complicated
Sailing Life on Jupiter

This Aluminum Boat Project Just Got Complicated

If you get value from our videos whether entertainment. education or inspiration show your appreciation by supporting our channel. ▶️Visit Our Website: https://www.sailinglifeonjupiter.com ▶️ SUPPORT US HERE 👇: JOIN our “PRIME” crew on PATR...
Was Changing Our Boat from 220V to 120V a Huge Mistake?
Sailing Life on Jupiter

Was Changing Our Boat from 220V to 120V a Huge Mistake?

Today we install a Victron MultiPlus Inverter as part of our big switch from 220V to 120V… and what should’ve been a simple swap turned into a full electrical overhaul. Out came the old Winston BMS wiring, new bus bars went in, a heat-damaged terminal...
Gave him something he’ll use every day… and definitely won’t forget. Happy birthday babe!
Sailing Life on Jupiter
POV: Can’t show up to our birthday dinner looking basic. #outfitcheck #birthdaycelebration #couple
Sailing Life on Jupiter
Everything We’ve Done to Our Aluminum Boat (So Far!)
Sailing Life on Jupiter

Everything We’ve Done to Our Aluminum Boat (So Far!)

If you get value from our videos whether entertainment. education or inspiration show your appreciation by supporting our channel. ▶️Visit Our Website: https://www.sailinglifeonjupiter.com ▶️ SUPPORT US HERE 👇: JOIN our “PRIME” crew on PATR...
Stuck at the Top: The Risky Halyard Retrieval
Sailing Life on Jupiter

Stuck at the Top: The Risky Halyard Retrieval

If you get value from our videos whether entertainment. education or inspiration show your appreciation by supporting our channel. ▶️Visit Our Website: https://www.sailinglifeonjupiter.com ▶️ SUPPORT US HERE 👇: JOIN our “PRIME” crew on PATR...
Stuck Halyards, Limited Options: This Could Get Dangerous
Sailing Life on Jupiter

Stuck Halyards, Limited Options: This Could Get Dangerous

Halyards stuck for years, no winch, no easy way up. Will a risky mast climb save us? ⛵️😬 If you get value from our videos whether entertainment. education or inspiration show your appreciation by supporting our channel. ▶️Visit Our Website: ht...
BougeRV 200w Anti-shading Flexible Mono Solar Panel
Sailing Life on Jupiter

BougeRV 200w Anti-shading Flexible Mono Solar Panel

Get Extra 8% Off with BOUGERV56 on BougeRV Amazon Store : https://bit.ly/4jAO1GB Get Extra 8% Off with BOUGERVLJ on Official site! https://bit.ly/456SHOw If you get value from our videos whether entertainment. education or inspiration show your apprecia...
Aluminum Corrosion: Here’s What We Found
Sailing Life on Jupiter

Aluminum Corrosion: Here’s What We Found

If you get value from our videos whether entertainment. education or inspiration show your appreciation by supporting our channel. ▶️Visit Our Website: https://www.sailinglifeonjupiter.com ▶️ SUPPORT US HERE 👇: JOIN our “PRIME” crew on PATR...
Aluminum Welding for Boat Projects
Sailing Life on Jupiter

Aluminum Welding for Boat Projects

Can a small TIG welder fix an aluminum boat? Four days aboard Jupiter² testing it. Four days working on Jupiter² and the progress is stacking up. From curdled coffee cream in Mexico to long days in the bilge, we’re cleaning compartments, prepping for ...
NEW CREW MEMBERS REVEAL ON JUPITER²
Sailing Life on Jupiter

NEW CREW MEMBERS REVEAL ON JUPITER²

Meet Bruce and Kim, the newest crew to join us aboard Jupiter! We first crossed paths years ago in Panama on a chocolate farm tour (yes, there was chocolate 😄), and now they’re back ready to help us prepare Jupiter for the long journey ahead toward Sp...
New year, new adventures! 🌊✨ Happy New Year from us to all of you! 🥂🎆 #newyear #welcome2026
Sailing Life on Jupiter

New year, new adventures! 🌊✨ Happy New Year from us to all of you! 🥂🎆 #newyear #welcome2026

New year, new adventures! 🌊✨ Wishing everyone a year filled with love, laughter, and unforgettable moments. Thank you for sharing this journey with us Happy New Year from us to all of you! 🥂🎆 #newyear #welcome2026 #fyp #viral #travel #everyo...
We Spent BIG on Our SailBoat This Holiday Season
Sailing Life on Jupiter

We Spent BIG on Our SailBoat This Holiday Season

We’re finally heading back to Jupiter after 8 months away. 🚚⚓ The truck is packed to the brim with tools, spare parts, and long-planned upgrades as we cross the border and return to the boatyard in Mexico. Customs, early mornings, and a whole lot of...
Christmas on Jupiter² 🎄⚓ Wrapping up the year and counting down to splash season.
Sailing Life on Jupiter
First time at the firing range and let’s just say, I did better than I thought.
Sailing Life on Jupiter
Some moments don’t need words just the view, the light, and the person you love.
Sailing Life on Jupiter

Some moments don’t need words just the view, the light, and the person you love.

Some moments don’t need words just the view, the light, and the person you love. Disclaimer: No copyright infringement is intended. #mounthood #timberline #oregon #snowday #couplegoals #travel #fypシ #everyoneシ゚
Planning an Epic Sailing Adventure California to Spain!
Sailing Life on Jupiter

Planning an Epic Sailing Adventure California to Spain!

Our plan to sail from California to Spain: four passages, one dream, and a huge adventure ahead. In this video, we share our full passage plan to relaunch Jupiter² and sail from Mexico all the way across the North Atlantic to Spain within a year. It’s ...
Traveling the world is fun… but traveling with someone who supports my dreams is everything.
Sailing Life on Jupiter

Traveling the world is fun… but traveling with someone who supports my dreams is everything.

Traveling the world is fun… but traveling with someone who supports my dreams is everything. Music credit : Dolia - Theme Music Polia, Theme Music, Song of Nature Sea Breeze Concerto | Honor of Kings Original Game Soundtrack • Timi Audio Lab #coupleg...
Epic water experiences, one click away.

Something AWESOME is coming!
Be the FIRST to know⛵

Sign up for exclusive updates and be the first to hear when we go live!
Get sneak peeks, exciting announcement, and special content straight to your inbox!

We don’t spam! Read our privacy policy for more info.


WeBoating
Logo
Shopping cart